Customization: | Available |
---|---|
Carbon Content: | High-Carbon |
Composition: | Carbon |
Still deciding? Get samples of US$ 1/Piece
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Property (Typical Value) |
TSK | GSK | Unit |
Apparent Density | ≥1.68 | ≥1.72 | g/cm3 |
Max Grain Size | ≤2 | ≤0.8 | mm |
Specific Electrical Resistivity | 8-10 | ≤8.5 | μΩm |
Flexural Strength | ≥12.5 | ≥15 | Mpa |
Compressive Strength | ≥28 | ≥35 | Mpa |
Porosity | ≤24 | ≤20 | % |
Ash value | ≤0.3 | ≤0.3 | % |
Property (Typical Value) |
HTG-4 | HTG-5 | Unit |
Apparent Density | ≥1.78 | ≥1.85 | g/cm3 |
Max Grain Size | ≤43 | ≤43 | µm |
Ash value | ≤500 | ≤500 | ppm |
Specific Electrical Resistivity | ≤12 | ≤10 | μΩm |
Flexural Strength | ≥35 | ≥40 | Mpa |
Compressive Strength | ≥60 | ≥70 | Mpa |
Shore Hardness | ≥40 | ≥45 | HSD |
Thermal Expansion (room temperature to 600ºC) | ≤4.5 | ≤4.4 | 10-6/ºC |
Property (Typical Value) |
HTD-5 | HTD-6 | HTD-7 | HTD-8 | HTD-9 | Unit |
Apparent Density | 1.85 | 1.90 | 1.82 | 1.90 | 1.82 | g/cm3 |
Max Grain Size | 13-15 | 8-10 | 8-10 | 8-10 | µm | |
Ash Content | ≤500 | ≤500 | ≤500 | ≤500 | ≤500 | ppm |
Purified ASH Content | 50 | 50 | 50 | 50 | 50 | ppm |
Specific Electrical Resistivity | 8-10 | 8-9 | 11-13 | 11-13 | 11-13 | μΩm |
Flexural Strength | 46 | 55 | 51 | 60 | 59 | Mpa |
Compressive Strength | 85 | 95 | 115 | 135 | 121 | Mpa |
Shore Hardness | 48 | 53 | 65 | 70 | 70 | HSD |
Thermal Expansion (room temperature to 600ºC) | 4.75 | 4.8 | 5.8 | 5.85 | 5.85 | 10-6/ºC |